Tag: Recycled Superalloy

Desktop Metal Qualifies Continuum’s Mar-M247 Recycled Superalloy
Resources

Desktop Metal Qualifies Continuum’s Mar-M247 Recycled Superalloy

free3dfilesnetSeptember 11, 2024

Desktop Metal qualifies Continuum’s Mar-M247, a 100% recycled superalloy, marking a new era in sustainable additive manufacturing. High performance meets eco-conscious innovation.